Alloy impurities of negative materials require PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC for iron removal
Время: 2024-11-23

eriz magnetic separator

Conventional synthesis methods such as solid phase method may result in inhomogeneity of cathode materials. When preparing iron oxide / carbon nanocomposite materials, the solid phase method may make the mixing of iron oxide and carbon uneven, which will affect the performance of the material, and thus affect the efficiency of iron removal. PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC Can solve this problem.


PTMS Electromagnetic Separator

The uneven material structure may lead to the difficult removal of iron in some areas of the element during the iron removal process. Because the PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC iron removal process requires iron to have a good diffusion channel inside the material, if the structure of the material is defective or uneven due to the synthesis method, these diffusion channels may be blocked or absent, thus reducing the efficiency of iron removal.


what is magnetic separation?

The presence of impurity elements may negatively affect the efficiency of iron removal. For lithium-ion battery cathode materials, impurities may change the crystal structure of the material or affect the ion diffusion path. Some metal impurities may form alloys or compounds with iron, making it more difficult to remove, requiring PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC to remove iron.

Contact: DELLA

Mob: +86-13929907491

sales@powtechina.com

Подписаться на новости

Foshan Powtech Technology Company Limited.

Адрес : No.9, Factory 2, Shijin Industry Park, Shishan Town, Nanhai District, Foshan City, Guangdong, China

Тел. : +86 -13929907491

Эл. адрес : sales@ptmsmagnet.com

Веб-сайт : https://www.dellamagnet.com

Авторское право © Foshan Powtech Technology Company Limited. Сохранить все права.   Sitemap   XML